This title is printed to order. This book may have been self-published. If so, we cannot guarantee the quality of the content. In the main most books will have gone through the editing process however some may not. We therefore suggest that you be aware of this before ordering this book. If in doubt check either the author or publisher’s details as we are unable to accept any returns unless they are faulty. Please contact us if you have any questions.
Im Rahmen des Forschungsprojektes Wandartige Tragwerke aus Stahlbeton wurden am Institut fur Baustatik und Konstruktion der Eidgenoessischen Technischen Hochschule Zurich Versuche an zehn quadratischen Stahl- betonscheiben durchgefuhrt. Die Versuche hatten zum Ziel, das Trag- und das Bruchverhalten von bewehrten Betonscheiben unter Normal- und Querkraftbeanspruchung, nachfolgend und im Bericht als Vertikal- und als Horizontal kraft bezeichnet, zu untersuchen. Die Scheiben wurden an ihrem oberen Rand belastet. Der untere Rand war eingespannt. Die Vertikal kraft blieb wahrend der Dauer eines Versuchs konstant. Die Horizontalkraft wurde stufenweise monoton oder zyk- lisch erhoeht, bis der Bruch eintrat. Die folgenden Groessen wurden als Versuchsparameter gewahlt: Ausfuh- rung der vertikalen Scheibenrander mit oder ohne Flansche, Aussparung in der Scheibendruckzone, Anordnung und Menge der Bewehrung sowie Betrag der Vertikalkraft. Fur die Untersuchung des Tragverhaltens wurden die aufgebrachten Krafte und Verschiebungen, die lokalen Deformationen der Betonoberflache und der Beweh- rungsstabe sowie die Rissweiten gemessen. Die Rissentwicklung wurde photographisch festgehalten. Die Versuchsergebnisse lassen sich wie folgt zusammenfassen: - Im allgemeinen trat der Bruch durch seitliches Aufspalten des Betons und durch Abplatzen der Ueberdeckung in der Druckecke der Scheibe auf. Die mit hoher Vertikal kraft beanspruchten Scheiben wiesen eine uber ihre ganze Lange gehende horizontale Zerstoerungszone auf. - Bei den Versuchen mit geringer Vertikal kraft bildeten sich die ersten Risse bei 20% bis 35% der Maximal- last. Die Scheiben mit hoher Vertikal kraft blieben bis zu einer Horizontalkraft von ungefahr zwei Dritteln des Maximums ungerissen.
$9.00 standard shipping within Australia
FREE standard shipping within Australia for orders over $100.00
Express & International shipping calculated at checkout
This title is printed to order. This book may have been self-published. If so, we cannot guarantee the quality of the content. In the main most books will have gone through the editing process however some may not. We therefore suggest that you be aware of this before ordering this book. If in doubt check either the author or publisher’s details as we are unable to accept any returns unless they are faulty. Please contact us if you have any questions.
Im Rahmen des Forschungsprojektes Wandartige Tragwerke aus Stahlbeton wurden am Institut fur Baustatik und Konstruktion der Eidgenoessischen Technischen Hochschule Zurich Versuche an zehn quadratischen Stahl- betonscheiben durchgefuhrt. Die Versuche hatten zum Ziel, das Trag- und das Bruchverhalten von bewehrten Betonscheiben unter Normal- und Querkraftbeanspruchung, nachfolgend und im Bericht als Vertikal- und als Horizontal kraft bezeichnet, zu untersuchen. Die Scheiben wurden an ihrem oberen Rand belastet. Der untere Rand war eingespannt. Die Vertikal kraft blieb wahrend der Dauer eines Versuchs konstant. Die Horizontalkraft wurde stufenweise monoton oder zyk- lisch erhoeht, bis der Bruch eintrat. Die folgenden Groessen wurden als Versuchsparameter gewahlt: Ausfuh- rung der vertikalen Scheibenrander mit oder ohne Flansche, Aussparung in der Scheibendruckzone, Anordnung und Menge der Bewehrung sowie Betrag der Vertikalkraft. Fur die Untersuchung des Tragverhaltens wurden die aufgebrachten Krafte und Verschiebungen, die lokalen Deformationen der Betonoberflache und der Beweh- rungsstabe sowie die Rissweiten gemessen. Die Rissentwicklung wurde photographisch festgehalten. Die Versuchsergebnisse lassen sich wie folgt zusammenfassen: - Im allgemeinen trat der Bruch durch seitliches Aufspalten des Betons und durch Abplatzen der Ueberdeckung in der Druckecke der Scheibe auf. Die mit hoher Vertikal kraft beanspruchten Scheiben wiesen eine uber ihre ganze Lange gehende horizontale Zerstoerungszone auf. - Bei den Versuchen mit geringer Vertikal kraft bildeten sich die ersten Risse bei 20% bis 35% der Maximal- last. Die Scheiben mit hoher Vertikal kraft blieben bis zu einer Horizontalkraft von ungefahr zwei Dritteln des Maximums ungerissen.